Georgia PAcific Tile Board Problem

We are using water based construction adhesive, per instructions. Our GP tile board is "growing" after we glue it up. As much as 1/8" on all sides. The problem is that the edge glue is holding and the sheets are buckling and splitting the glue film. It is buckling even on smaller 2'x3' sections.

The panels were put into the room 24 hours before installation.

Why is the tile board swelling and getting these "bubbles"?

Any help or tips greatly appreciated.


FL
 
  #2  
Old 08-25-07, 04:10 PM
H
Member
Join Date: Jan 2006
Location: USA
Posts: 3,280
Received 9 Upvotes on 9 Posts
Not sure what your doing. Is this a backerboard that you apply ceramic tile too or is this some kinda finished product that looks like ceramic tile?
 
 